Testing Products for ASTM D6484
APP-D6484
Application Insight:
Compression After Impact: Tests how much a hole (damage) reduces the crushing strength of a wing panel.
Compliant Hardware Solution
612-1000-630
This machine has been validated to meet the specific requirements of this standard.
View Machine DetailsRegulatory & Test Details
| App Id | APP-D6484 |
|---|---|
| App Standard | ASTM D6484 |
| Standard Organization | ASTM |
| Test Type | Compression |
| Material Type | Composite |
| Specimen Type | Plate with 6mm Hole |
| Industry Type | Aerospace / Composites |
| Min Force Kn | 100 |
| Max Force Kn | 1 |
| Min Spd Mm/m | 2 |
| Max Spd Mm/m | 2 |
| Expert Spd | Open-hole compression composite. |
| Mach Recommend | 612-1000-630 |
| Pointer App Software | N-ASTM-D6484 |
| Pointer Fixture Family | G-ASTM-D6484 |
| Pointer Strain Family | E-ASTM-D6484 |
Implementation Commentary
This is one of the hardest tests to perform; the fixture often weighs more than the specimen.