ASTM A370 Test Guide: Tensile Testing for Metals
TensileAlways use an extensometer rated for high-velocity shocks, and remove it immediately after yield if testing to failure.
Browse validated testing configurations. Filter by regulatory standard, material type, or force requirements.
34 items found
Always use an extensometer rated for high-velocity shocks, and remove it immediately after yield if testing to failure.
Grind the chisel edge to the exact specified angle and sharpen regularly to maintain uniform shear force application.
Clean and prime the substrate blocks precisely according to the manufacturer’s spec to isolate true sealant engineering limits.
When performing the perpendicular tensile test, use a high-strength epoxy to bond the metal blocks uniformly across the fiber face.
Always sandblast and solvent-wipe the steel loading plates to bare metal immediately before applying epoxy to prevent premature bond line…
Cure the bonded block assembly under a uniform dead-weight load to ensure a perfectly flat, parallel adhesive layer.
Always roll the tape onto the steel plate with a standardized mechanical roller at a uniform speed to eliminate manual…
Always insert spacer shims equal to the coupon thickness into the grips to guarantee a perfectly straight axial line of…
Always apply the static bending load to the natural molded face of the panel, and cross-reference thickness variations down to…
Always apply the exact standard-specified pre-tension (typically 0.5 cN / tex) to remove structural slack before zeroing strain metrics.
Clean the stainless steel probe tip with reagent-grade toluene or isopropyl alcohol and a lint-free wipe before every single stroke.
Always insert thickness-matching spacers into the grip jaws behind the specimen tabs to keep the bond line perfectly collinear with…
Measure notch separation distance with an optical micrometer to the nearest 0.05mm to secure perfect shear area parameters.
Meticulously clean the stainless steel test plate with diacetone alcohol or n-heptane and a lint-free wipe before every single strip…
You must gather both longitudinal and transverse strain simultaneously; in-plane shear strain equals axial strain minus transverse strain.
Verify that the two lap joints are identical in surface area and bond line thickness to protect the mechanical symmetry…
Verify that the machined notches pass exactly halfway through the specimen thickness to isolate a clean, center-plane shear field.
Never use standard manual screw grips; vulcanized rubber narrows drastically under tension and requires self-adjusting pneumatic jaws.
Meticulously document the exact failure mode split: R (Rubber Failure), RC (Rubber-Cement), CP (Cement-Primer), or M (Metal Interface).
Store and condition tape rolls at standard atmospheric limits for exactly 24 hours prior to slitting or testing to equalize…