ASTM A370 Test Guide: Tensile Testing for Metals
TensileAlways use an extensometer rated for high-velocity shocks, and remove it immediately after yield if testing to failure.
Browse validated testing configurations. Filter by regulatory standard, material type, or force requirements.
22 items found
Always use an extensometer rated for high-velocity shocks, and remove it immediately after yield if testing to failure.
Clean and prime the substrate blocks precisely according to the manufacturer’s spec to isolate true sealant engineering limits.
When performing the perpendicular tensile test, use a high-strength epoxy to bond the metal blocks uniformly across the fiber face.
Cure the bonded block assembly under a uniform dead-weight load to ensure a perfectly flat, parallel adhesive layer.
Grind the loaded ends of the sandwich panel flat and perpendicular to the facings within 0.02mm to eliminate edge stress…
Always use a direct-contact deflectometer setup to measure core deflection; crosshead travel includes platen-seating errors.
Always apply the static bending load to the natural molded face of the panel, and cross-reference thickness variations down to…
Cut the foam blocks with a precision bandsaw or hot-wire setup to ensure the loading faces are perfectly flat and…
Always apply the exact standard-specified pre-tension (typically 0.5 cN / tex) to remove structural slack before zeroing strain metrics.
Always bond back-to-back strain gauges on every specimen to actively compute and document real-time out-of-plane bending percentages.
Always execute the three required structural pre-flex cycles to 75% deflection before recording official IFD force data.
Never use standard manual screw grips; vulcanized rubber narrows drastically under tension and requires self-adjusting pneumatic jaws.
Store and condition tape rolls at standard atmospheric limits for exactly 24 hours prior to slitting or testing to equalize…
Calibrate the precise initial distance between the roller axes using a solid reference spacer to guarantee an exact baseline loop…
Coat the internal walls of the confinement fixture with a micro-thin layer of silicone grease or mineral oil to completely…
Apply a thin, uniform layer of silicone oil or petroleum jelly to platens to minimize interfacial friction coefficients.
Inspect the internal perimeter of the drilled hole under a microscope before testing; any evidence of fiber fraying or ply…
Always measure real specimen cross-section thickness at 3 distinct points before clamping; do not rely on nominal molded values.
Always verify that the upper spherically seated platen is unlocked and free to float during alignment, then locked or allowed…
Always apply a minimal, uniform pre-load (~0.5 cN / tex) prior to starting the test loop to eliminate structural slack…