ASTM A370 Test Guide: Tensile Testing for Metals
TensileAlways use an extensometer rated for high-velocity shocks, and remove it immediately after yield if testing to failure.
Browse validated testing configurations. Filter by regulatory standard, material type, or force requirements.
28 items found
Always use an extensometer rated for high-velocity shocks, and remove it immediately after yield if testing to failure.
Clean and prime the substrate blocks precisely according to the manufacturer’s spec to isolate true sealant engineering limits.
When performing the perpendicular tensile test, use a high-strength epoxy to bond the metal blocks uniformly across the fiber face.
Always sandblast and solvent-wipe the steel loading plates to bare metal immediately before applying epoxy to prevent premature bond line…
Cure the bonded block assembly under a uniform dead-weight load to ensure a perfectly flat, parallel adhesive layer.
Always insert spacer shims equal to the coupon thickness into the grips to guarantee a perfectly straight axial line of…
Always apply the static bending load to the natural molded face of the panel, and cross-reference thickness variations down to…
Always apply the exact standard-specified pre-tension (typically 0.5 cN / tex) to remove structural slack before zeroing strain metrics.
Always insert thickness-matching spacers into the grip jaws behind the specimen tabs to keep the bond line perfectly collinear with…
Measure notch separation distance with an optical micrometer to the nearest 0.05mm to secure perfect shear area parameters.
You must gather both longitudinal and transverse strain simultaneously; in-plane shear strain equals axial strain minus transverse strain.
Verify that the two lap joints are identical in surface area and bond line thickness to protect the mechanical symmetry…
Verify that the machined notches pass exactly halfway through the specimen thickness to isolate a clean, center-plane shear field.
Never use standard manual screw grips; vulcanized rubber narrows drastically under tension and requires self-adjusting pneumatic jaws.
Store and condition tape rolls at standard atmospheric limits for exactly 24 hours prior to slitting or testing to equalize…
Ensure the shearing tool blade rests perfectly flat against the step edge and is collinear with the bond line plane…
Calibrate the precise initial distance between the roller axes using a solid reference spacer to guarantee an exact baseline loop…
Always use a calibrated 4.5kg weighted roller running at a consistent speed to mate the hook and loop sections; never…
Always apply two cross-axial strain gauges mounted at $pm$45 degrees relative to the loading axis within the notch zone to…
Inspect the internal perimeter of the drilled hole under a microscope before testing; any evidence of fiber fraying or ply…